When the carbon content of the weld is 0.55%, the plasticity of the weld almost disappears and becomes a very brittle material, and this brittleness cannot be eliminated by post-weld heat treatment.
Mechanical treatment: mainly includes shot blasting method and shot peening method. Shot blasting is a method of using centrifugal force to accelerate projectiles and project them to the workpiece ...